Nama Produk SSAW (Dikimpal Arka Terendam Lingkaran)
Paip besi
Penggunaan Digunakan untuk penghantaran cecair tekanan rendah,
seperti air, gas dan minyak.
API Standard 5L PSL1/ PSL2 , ASTM A252, EN10219,
AWWA C200, ASTM A53, BS, JIS, dll...
ASTM A 53 Gr. A, Gr B, Gr C, Gr.D
API 5L A, B, X42, X46, X52, X56, X60, X65 X70
GB/T9711 L175, L210, L245, L290, L320, L360,
L290, L320, L360, L390, L415, L450, L485, L555
ASTM A252 Gr.1 Gr.2 Gr.3
Penerangan Produk
| Nama Produk | SSAW paip keluli lingkaran |
| Panjang Paip | 6-12m |
| O.D | 219mm-3000mm |
| W.T | 5mm{1}}mm |
| Teknologi | SAW |
| Gred |
API 5L PSL1 PSL2 x42, x46, x52, x56, x60, x70 |
| bahan | Q235, Q345, St37, St37-2, A53, Mn16, dll |
| Permohonan | paip air, cerucuk keluli, paip minyak dan gas, saluran paip keluli |
| Rawatan permukaan | lukisan kosong, berminyak, hitam, bergalvani, salutan 3pe anti-menghakis, dsb |
| Sijil | API 5L, ISO9001:2015, ISO14001, OHSAS18001 |
| Terma pembayaran | T/T, L/C, Western Union, Tunai, dsb |